well, it's definitely "proud" above the dent area... i don't know how to specify, maybe 1/8 to 3/16 extra.. cheesegraters are usually good on large shallow dent areas, like on a door.. where doing it in one app is preferable.. not EVERY time you do mud work...
and it works well with body fillers, fiberglass fillers, not as much..
don't worry about it, get a sand block, some 36 and 80 grit... you wann rip it close with 36, just a tad high, then take out the 36 scratches with 80 grit and that leaves ya just about right...
and it works well with body fillers, fiberglass fillers, not as much..
don't worry about it, get a sand block, some 36 and 80 grit... you wann rip it close with 36, just a tad high, then take out the 36 scratches with 80 grit and that leaves ya just about right...


yeah, sure use 1970's nitrostain putty, wheren't too many shrinking issues with that crap.. frikkin moron, try joining at least the 80's... 